Stainless steel grades table
Heat-resistant steel is resistant to factors such as hot gases, burning products, molten salts and metals at temperatures exceeding 550ºC. Depending on chemical composition, the following steels can be identified: ferritic steels, austenitic steels, nickel-based steels.
Heat-resistant steels are used for industrial furnace construction, heat-resistant components of steam boilers, components of plastics dryers, in chemical industry, in power plants, in rolling mills for pipes and mill guides.
EN | DIN | AISI | PN | C | Si | Mn max | P max | S max | Al | Cr | Ni | Heat resistance in air oC |
1.4713 | X 10 Cr Al 7 | - | ≤ 0,12 | 0,5 - 1,0 | 1 | 0,04 | 0,03 | 0,5-1,0 | 6,0-8,0 | - | 800 | |
1.4720 | X 7 CrTi 12 | 409 | ≤ 0,08 | ≤ 0,1 | 1 | 0,04 | 0,03 | - | 10,5-12,5 | - | 800 | |
1.4724 | X 10 CrAl 13 | - | H13JS | 0,12 | 0,7 - 1,4 | 1 | 0,04 | 0,03 | 0,7-1,2 | 12,0-14,0 | - | 850 |
1.4742 | X 10 CrAl 18 | - | H18JS | 0,12 | 0,7 - 1,4 | 1 | 0,04 | 0,3 | 0,7-1,2 | 17,0-19,0 | - | 1000 |
1.4749 | X 18 CrN 28 | 446 | H25T | 0,15-0,20 | Max. 1,0 | 1.0 | 0,04 | 0,03 | - | 24,0-29,0 | - | 1100 |
1.4762 | X10 CrAl 24 | (TP 446) | H24JS | ≤ 0,12 | 0,7 - 1,4 | 1 | 0,04 | 0,03 | 1,2-1,7 | 23,0-26,0 | - | 1150 |
1.4828 | X 15 CrNiSi 20 12 | 309 | H20N12S2 | ≤ 0,20 | 1,5 - 2,5 | 2 | 0,045 | 0,03 | - | 19,0-21,0 | 1,0-13,0 | 1050 |
1.4841 | X 15 CrNiSi 25 20 | 314 | H25N20S2 | ≤ 0,20 | 1,5 - 2,5 | 2 | 0,045 | 0,03 | - | 24,0-26,0 | 19,0-22,0 | 1150 |
1.4845 | X 12 CrNI 25 21 | 310 S/H | H23N18 | ≤ 0,15 | ≤ 0,75 | 2 | 0,045 | 0,03 | - | 24,0-26,0 | 19,0-22,0 | 1050 |
1.4876 | X 10 NiCrAlTi 32 20 | - | ≤ 0,12 | ≤ 0,1 | 2 | 0,045 | 0,02 | 0,15-0,6 | 19,0-23,0 | 30,0-34,0 | 1100 | |
1.4878 | X12 CrNiTi 18 9 | 321 | 1H18N9T | ≤ 0,12 | ≤ 1,0 | 2 | 0,045 | 0,03 | - | 17,0-19,0 | 9,0-12,0 | 850 |
2.4816 | NiCr 15 Fe | - | 0 | 0,5 | 1 | 0,015 | 0,015 | - | 14-17 | - | 1050 | |
2.4851 | NiCr 23 Fe | - | 0,1 | 0,5 | 1 | 0,02 | 0,015 | 1-1,7 | 21-25 | 58-63 | 1150 |